Further tests showed that the samples prepared at 60 °C did not deliver PS polymer spheres. Based on the DLS measurements, the sample has a broad dimensions distribution which may be spelled out by the slow initiation action which allows for your formation of a little quantity of nuclei that grow in measurement, whilst new KPS radicals initiated n… Read More